Critical cooling rate for the glass formation of ferromagnetic Fe40Ni40P14B6 alloy

Physics – Condensed Matter – Materials Science

Scientific paper

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

23 pages, 3 figures, 1 table

Scientific paper

Bulk ferromagnetic amorphous Fe-Ni-P-B alloys in rod shape were formed by a rapid solidification technique. The largest amorphous specimen prepared had a diameter of ~2.5 mm and the corresponding cooling rate for the glass formation of this alloy system in our experiment can be estimate to be around 492.4 K/s by the method of finite-difference numerical calculation. This value is on the same order of magnitude as the critical cooling rate Rc of Fe40Ni40P14B6 alloy estimated by the method of constructing the continuous-cooling-transformation (CCT) curve. It is indicated that the heterophase impurities have been eliminated well in our experiment.

No associations

LandOfFree

Say what you really think

Search LandOfFree.com for scientists and scientific papers. Rate them and share your experience with other people.

Rating

Critical cooling rate for the glass formation of ferromagnetic Fe40Ni40P14B6 alloy does not yet have a rating. At this time, there are no reviews or comments for this scientific paper.

If you have personal experience with Critical cooling rate for the glass formation of ferromagnetic Fe40Ni40P14B6 alloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Critical cooling rate for the glass formation of ferromagnetic Fe40Ni40P14B6 alloy will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFWR-SCP-O-576569

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.