Ordered arrays of magnetic nanowires are commonly synthesized by electrodeposition in nanoporous alumina templates. Due to their dense packing, strong magnetostatic interactions prevent the manipulation of wires individually. Using atomic layer deposition we reduce the diameter of the pores prior to electrodeposition. This reduces magnetostatic interactions, yielding fully remanent hysteresis loops. This is a first step towards the use of such arrays for magnetic racetrack memories.
Cagnon Laurent
Col Sandrine Da
Darques Michael
Fruchart Olivier
No associations
LandOfFree
Reduction of magnetostatic interactions in self-organized arrays of nickel nanowires using atomic layer deposition does not yet have a rating. At this time, there are no reviews or comments for this scientific paper.
If you have personal experience with Reduction of magnetostatic interactions in self-organized arrays of nickel nanowires using atomic layer deposition, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Reduction of magnetostatic interactions in self-organized arrays of nickel nanowires using atomic layer deposition will most certainly appreciate the feedback.
Profile ID: LFWR-SCP-O-456146