Nanoindentation of bilayer graphene is studied using molecular dynamics simulations. We compared our simulation results with those from elasticity theory as based on the nonlinear F\"{o}ppl-Hencky equations with rigid boundary condition. The force deflection values of bilayer graphene are compered to those of monolayer graphene. Young's modulus of bilayer graphene is estimated to be 0.8 TPa which is close to the value for graphite. Moreover, an almost flat bilayer membrane at low temperature under central load has a 14$%$ smaller Young's modulus as compared to the one at room temperature.
Neek-Amal Mehdi
Peeters François M.
No associations
LandOfFree
Nanoindentation of a circular sheet of bilayer graphene does not yet have a rating. At this time, there are no reviews or comments for this scientific paper.
If you have personal experience with Nanoindentation of a circular sheet of bilayer graphene, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nanoindentation of a circular sheet of bilayer graphene will most certainly appreciate the feedback.
Profile ID: LFWR-SCP-O-497296