A method to treat the surface of Nb is described which potentially can improve the performance of superconducting RF cavities. We present tunneling and x-ray photoemission spectroscopy (XPS) measurements at the surface of cavity-grade niobium samples coated with a 3 nm alumina overlayer deposited by Atomic Layer Deposition (ALD). The coated samples baked in ultra high vacuum (UHV) at low temperature reveal at first degraded superconducting surface. However, at temperatures above 450C, the tunneling conductance curves show significant improvements of the superconducting density of states (DOS) compared with untreated surfaces.
Antoine Ch.
Cooley L.
Elam J.
Gray Kenneth E.
Moore Joshua
No associations
LandOfFree
Improvement and protection of niobium surface superconductivity by Atomic Layer Deposition and heat treatment does not yet have a rating. At this time, there are no reviews or comments for this scientific paper.
If you have personal experience with Improvement and protection of niobium surface superconductivity by Atomic Layer Deposition and heat treatment, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Improvement and protection of niobium surface superconductivity by Atomic Layer Deposition and heat treatment will most certainly appreciate the feedback.
Profile ID: LFWR-SCP-O-281164