The effects of reduced pressure and flow rates were determined on the
thermal analysis of synthetic lepidocrocite using a modified
differential scanning calorimeter in support of the Mars '98 Lander
Thermal and Evolved Gas Analyzer (TEGA).

No associations

LandOfFree

Say what you really think

Search LandOfFree.com for scientists and scientific papers. Rate them and share your experience with other people.

Rating

Differential Scanning Calorimetry of Hydrous Minerals Under Mars-like Conditions: Calibration Studies for the Mars '98 Lander Thermal and Evolved Gas Analyzer does not yet have a rating. At this time, there are no reviews or comments for this scientific paper.

If you have personal experience with Differential Scanning Calorimetry of Hydrous Minerals Under Mars-like Conditions: Calibration Studies for the Mars '98 Lander Thermal and Evolved Gas Analyzer, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Differential Scanning Calorimetry of Hydrous Minerals Under Mars-like Conditions: Calibration Studies for the Mars '98 Lander Thermal and Evolved Gas Analyzer will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFWR-SCP-O-843239

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.