Magnetite (Fe3O4) films were fabricated on MgAl2O4 (001) single crystal substrates by pulsed laser deposition. In-plane and out-of-plane lattice constants were determined by X-ray diffraction. The apparent Poisson's ratio was determined as the negative ratio of the out-of-plane to in-plane strains. The results show that (i) the determination of Poisson's ratio by this method is only reliable for fully strained films and (ii) Poisson's ratio = 0.3 along the <100> direction is positive for this archetypal ferrite. Fe3O4 films grown on MgAl2O4 (001) are not auxetic.

No associations

LandOfFree

Say what you really think

Search LandOfFree.com for scientists and scientific papers. Rate them and share your experience with other people.

Rating

Are magnetite (Fe3O4) films on MgAl2O4 auxetic? does not yet have a rating. At this time, there are no reviews or comments for this scientific paper.

If you have personal experience with Are magnetite (Fe3O4) films on MgAl2O4 auxetic?, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Are magnetite (Fe3O4) films on MgAl2O4 auxetic? will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFWR-SCP-O-185673

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.