Ta (100 nm) / NdFeB (5 $\mu$m) / Ta (100 nm) films have been deposited onto Si substrates using triode sputtering (deposition rate ~ 18 $\mu$m/h). A 2-step procedure was used : deposition at temperatures up to 400 C followed by ex-situ annealing at higher temperatures. Post-deposition annealing temperatures above 650 C are needed to develop high values of coercivity. The duration of the annealing time is more critical in anisotropic samples deposited onto heated substrates than in isotropic samples deposited at lower temperatures. For a given set of annealing conditions (750 C/ 10'), high heating rates (≥ 2000 C / h) favour high coercivity in both isotropic and anisotropic films. The shape and size of Nd2Fe14B grains depend strongly on the heating rate.

No associations

LandOfFree

Say what you really think

Search LandOfFree.com for scientists and scientific papers. Rate them and share your experience with other people.

Rating

Evolution of magnetic and microstructural properties of thick sputtered NdFeB films with processing temperature does not yet have a rating. At this time, there are no reviews or comments for this scientific paper.

If you have personal experience with Evolution of magnetic and microstructural properties of thick sputtered NdFeB films with processing temperature, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Evolution of magnetic and microstructural properties of thick sputtered NdFeB films with processing temperature will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFWR-SCP-O-711116

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.