Mechanism of pyroxene and amphibole weathering--I. Experimental studies of iron-free minerals

Physics

Scientific paper

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

29

Scientific paper

The short term (2-40 days) dissolution of enstatite, diopside, and tremolite in aqueous solution at low temperatures (20-60°C) and pH 1-6 has been studied in the laboratory by means of chemical analyses of reacting solutions for Ca 2+ , Mg 2+ , and Si(OH) 4 and by the use of X-ray photoelectron spectroscopy (XPS) for detecting changes in surface chemistry of the minerals. All three minerals were found to release silica at a constant rate (linear kinetics) providing that ultrafine particles, produced by grinding, were removed initially by HF treatment. All three also underwent incongruent dissolution with preferential release of Ca and/or Mg relative to Si from their outermost surfaces. The preferential release of Ca, but not Mg for diopside at pH 6 was found by both XPS and solution chemistry verifying the theoretical prediction of greater mobility of cations located in M 2 structural sites. Loss mainly from M 2 sites also explains the degree of preferential loss of Mg from enstatite at pH 6; similar structural arguments apply to the loss of Ca and Mg from the surface of tremolite. In the case of diopside and tremolite initial incongruency was followed by essentially congruent cation-plus-silica dissolution indicating rapid formation of a constant-thickness, cation-depleted surface layer. Cation depletion at elevated temperature and low pH (~ 1) for enstatite and diopside was much greater than at low temperature and neutral pH, and continued reaction resulted in the formation of a surface precipitate of pure silica as indicated by solubility calculations, XPS analyses, and scanning electron microscopy. From XPS results at pH 6, model calculations indicate a cation-depleted altered surface layer of only a few atoms thickness in all three minerals. Also, lack of shifts in XPS peak energies for Si, Ca, and Mg, along with undersaturation of solutions with respect to all known Mg and Ca silicate minerals, suggest that cation depletion results from the substitution of hydrogen ion for Ca 2+ and/or Mg 2+ in a modified silicate structure and not from the precipitation of a new, radically different surface phase. These results, combined with findings of high activation energies for dissolution, a non-linear dependence on a H + for silica release from enstatite and diopside, and the occurrence of etch pitting, all point to surface chemical reaction and not bulk diffusion (either in solution or through altered surface layers) as the rate controlling mechanism of iron-free pyroxene and amphibole dissolution at earth surface temperatures.

No associations

LandOfFree

Say what you really think

Search LandOfFree.com for scientists and scientific papers. Rate them and share your experience with other people.

Rating

Mechanism of pyroxene and amphibole weathering--I. Experimental studies of iron-free minerals does not yet have a rating. At this time, there are no reviews or comments for this scientific paper.

If you have personal experience with Mechanism of pyroxene and amphibole weathering--I. Experimental studies of iron-free minerals, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Mechanism of pyroxene and amphibole weathering--I. Experimental studies of iron-free minerals will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFWR-SCP-O-744191

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.